Title: Thermoelectric power factor for polyaniline/molybdenum trioxide composites
Authors: Anilkumar K.R
Parveen A
Badiger G.R
Ambika Prasad M.V.N.
Keywords: composites
polyaniline
Seebeck coefficient
Thermoelectric power factor
Issue Date: 2009
Citation: Ferroelectrics , Vol. 386 , 1 , p. 88 - 93
Abstract: The results of thermoelectric power (TEP), power factor and Seebeck coefficient of conducting polyaniline molybdenum trioxide (PANI/MoO3) composites of different weight percentages (10, 20, 30, 40 and 50wt %) has been reported. The results are supported by the theory of coupled transport equations of heat and electricity in metals. It is observed that even though the Seebeck coefficient decreases with doping, the power factor increases with increase in electrical conductivity. The conductivity results lie between 10-5 and 10-3 S/cm from 0 wt% to 50wt% of MoO3 in PANI respectively match with that of conventional semiconductors. Copyright ©Taylor & Francis Group, LLC.
URI: 10.1080/00150190902961801
http://gukir.inflibnet.ac.in:8080/jspui/handle/123456789/5273
Appears in Collections:1. Journal Articles

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.